Green Peel Bond Procedure at the Corrugator

Category:

Description

TAPPI UM 822 – Green Peel Bond Procedure at the Corrugator

This procedure is to provide basic instructions for subjective testing of the corrugated bond at both the single facer and doublebacker glue lines. The combined board should be allowed to cool for approximately 10 minutes at the dry end of the corrugator before evaluation.